How to configure the coating for precision casting

Your current location: Home >> News >> Company news

How to configure the coating for precision casting

Release date:2017-10-09 Author: Click:

How to configure the coating for precision casting

There are some curious customers is really an interesting thing, recently we are also interested in precision casting coating preparation method, then our company to everyone to explain it:

Physical and chemical parameters of silica sol mainly include SIO2 content, density, Na2o content, PH value, kinematic viscosity, colloidal particle diameter, etc. These physical and chemical parameters mainly affect the strength of precision cast shell, the stability of coating and the powder to liquid ratio of coating.

Because it is very difficult for precision casting enterprises to test these physical and chemical parameters, on the one hand, it is necessary to strengthen the selection, evaluation and confirmation of suppliers. On the other hand, silicon sol of different specifications should be selected for surface layer and back layer, s-830 silicon sol for surface layer and s-1430 silicon sol for back layer.The quality of the casting is directly affected by the method of coating preparation in precision casting.Precision casting

The coating preparation usually adds silica sol first, then adds wetting agent to mix well, adds refractory powder in the stirring, and finally adds defoaming agent.To ensure the quality of coating, surface coating are all new material, stirring time should be more than 24 hours to use, such as part of new ingredients, mixing time can be shortened to twelve hours. A transition layer and back layer of paint mixing time can be less than the surface coating, all for the new match paint, stirring time is more than ten hours, part for the new timing, mixing time can be shorten the half.Match the paint if not used, should be sealed to prevent evaporation of water.

Above is precision casting coating preparation method, if you need precision casting, you can choose to consider our company.


This article URL:http://cgik.cn/en/news/350.html

Related tags:精密鑄造件

Recently Viewed:

share 一鍵分享
美女AAA久| 亚洲啪啪小视频| 在线播放免费播放av片| 开心激情五月婷婷丁香| 摸人人| 精品国产乱码久久久软件下载| 亚洲国产黑人| 亚洲最新另类| 亚洲产国偷v产偷v自拍涩爱 | AAA精品国产| 少妇高潮毛片色欲AVA片| 精品少如| 夜夜操,狠狠操| 一区二区无码久久| 亚洲精品人成网线在播放va| 国产av美女被操| 国产不卡中文有色| 精品精品精品| 波多野结衣一区二区三区av高清| 男女涩涩免费观看| 色五月五月丁香| 亚洲天堂无码在线| 欧美二三区| 日本a级特大片| 免费观看欧洲在线视频| 第一次的人妻| 欧美国产91| 日韩在线播放网站| 欧美1区 2区3区| 国产精品久久久久久久裸模| 免费无码又爽又刺激高潮的APP| 四房色播在线视频| 精品乱码一区小说| 好紧好湿视频| 中国成熟妇女毛茸茸| 精品久久久久免费| 日韩一区三区电影| 欧美日韩成人av欧美| av77777| 日韩免费精彩视频| 日韩欧美视频免费h|